15CrMo kotel cev
Apr 18, 2024
Debelina: 8MM do 250 MM
Širina: 1500mm do 4050mm
Dolžina: 3000mm do 15000mm
15CrMo zlitina jeklo cev kemična sestava |
|||||
| Razred | The Element Max (%) | ||||
| C | Si | Mn | P | S | |
| 15CrMo | 0.12-0.18 | 0.17-0.37 | 0.40-0.70 | 0.035 | 0.035 |
15CrMo zlitina cev Mehanska Lastnost |
||||
| Razred | Debelina | Donos | Natezno | HB |
| 15CrMo | Mm | Min Mpa | Mpa | HB |
| 6-50 | 295 | 440 | ||
| 50-200 | 295 | 440 | ||
15CrMo zlitina kotel cev zunanjost premer & toleranca
|
Vroče valjano |
Zunanjost Premer, mm |
||
|
Napreden |
|||
|
OD manj kot ali enako to to 54 |
±0.50mm |
±0.30mm |
|
|
54<OD Manj than or equal to to 325 |
±1% |
±0.75% |
|
|
OD>325 |
±1% |
- |
|
|
Hladno narisano |
Zunanjost Premer, mm |
||
|
Navaden |
Napreden |
||
|
OD Manj kot ali enako to do 25,4 |
±0.15mm |
- |
|
|
25.4<OD manj than or equal to 40 |
±0.20mm |
- |
|
|
40<OD Manj than or equal to to 50 |
±0.25mm |
- |
|
|
50<OD Manj than or equal to 60 |
±0.30mm |
- |
|
|
OD>60 |
±0.75% |
±0.50% |
|
15CrMo jeklo cev Stena debelina & toleranca
|
Vroče valjano |
Stena debelina, mm |
Tolerance |
|
|
Navaden |
Napreden |
||
|
WT Manj kot ali enako to 20 |
+15%/-10% |
±10% |
|
|
WT>20 |
+12.5%/-10% |
±10% |
|
|
Hladno narisano |
Stena debelina, mm |
Tolerance |
|
|
Navaden |
Napreden |
||
|
WT manj kot ali enako do do 3.0 |
±0.30mm |
±0.20mm |
|
|
WT>3 |
±10% |
±7.5% |
|
15CrMo nizka zlitina jeklo cev

GNEE Group specializes in supplying 15CrMo alloy steel pipes. Our products comply with API 5L and API 5CT standards, ASTM A252, ASTM A53 and ASTM A500 standards, and EN10217 and EN10219 standards, and are ISO90012008 certified. If you have any needs, please describe the product specifications you need and we will quote you as soon as possible.